Steel 1.2345 - USD-H

1.2345 - USD-H:
higher temper resistance and hardenability.

1.2345 – USD-H steel is a hot-work tool steel with increased carbon content for increased resistance to wear, higher temper resistance and hardenability.

Properties of steel type 1.2345 – USD-H
 
  • Increased carbon content .
  • Increased resistance to wear .
  • Higher temper resistance and hardenability.
The most common applications for steel type 1.2345 – USD-H are:
 
  • Cold and hot shear blades.
  • Forging dies.
  • Rollers for pipe manufacturing.

Physical properties of 1.2345 - USD-H steel

Temperature in °C20-10020-20020-400
Thermal expansion in 10-6m/m x K11.512.513.1
Temperature in °C20200400
Thermal conductivity in W/m x K25.026.727.3
Temperature in °C20
Density in g/cm37.73
Temperature in °C20
E module in GPa215

Heat treatment

Soft annealingTemperature: 760 – 810 °C, 4 – 6 hrs
Cooling: slow furnace cooling
Hardness: max. 240 HB
HardeningTemperature: 1010 – 1040 °C
Cooling Oil or polymer cooling or vacuum hardening
TemperingTemperature: 520 – 620 °C
Hardness: see tempering curve
NitridingPossible
Preheat before useTemperature: 150 – 350 °C

Graphs and datasheets for 1.2345 - USD-H

1.2345 USD-H steel